Formad Madencilik

Çalışmalarımızdan Görüntüler












Maden Sahamızdaki Madenlere Ait Teknik Analiz Raporu
KAOLİN

CODE F-T.257 F-T.257/Ç F-T.257/1 F-T.257/H
CHEMICAL
ANALYSIS
(%)

Min Max Min Max Min Max. Min Max
L.O.I 10.50 13.00 4.50 6.50 11.00 13.00 7.00 9.00
SiO2 49.00 55.00 72.00 78.00 49.00 53.00 64.00 72.00
Al2O3 30.00 34.00 14.00 17.00 32.00 34.00 18.00 24.00
Fe2O3
1.40
0.40
0.80
1.10
TiO2
0.50
0.40
0.50
0.50
CaO
0.50
0.70
0.50
0.50
MgO
0.25
0.20
0.20
0.20
Na2O
0.12
0.50
0.12
0.30
K2O
0.20
0.50
0.20
0.50
SO3
0.50
0.50
0.50
0.50
RATIONAL
ANALYSIS
(%)
Kaolinite 80.00 36.00 82.50 50.50
Na-Feldspar 1.00 4.50 1.00 2.50
K-Feldspar 1.20 3.00 1.20 3.00
Free Quartz 15.00 54.50 11.00 41.00
Others 2.80 2.00 4.30 3.00
PARTICLE
SIZE
CRUSHED SIZE ACCORDING TO CUSTOMER'S REQUIREMENT
(-50 mm, -25 mm, -10 mm, -4 mm)
GROUND SIZE ACCORDING TO CUSTOMER'S REQUIREMENT
(-1000 µ, -500 µ, -100 µ, -63 µ)
FIRING
PROPERTIES
Temperature
(°C)
1250 1250 1250 1140 1160
Colour White White White Cream
CASTING
DATA
Pulp Density
(gr/lt)
1750 1730

Optimum
Electrolyte
(%)
0.15

0.30

-

0.20
Max.Solid
Conc. (%)
70.00

69.00


Casting Rate
(mm2/min)
1.50

3.00

1.50

3.00
Elecirolyte used is 38 Baume Na2SiO3

Telefon: (0266) 221 18 07 - Faks: (0266) 221 00 87
Site Tasarım ve Hosting